Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 100 °C |
66.7 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics POM-C Acetal Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 - 100 °C |
66.7 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon FEP Fluorinated Ethylene Propylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM E831 |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | DIN 52328 |
Isoflon PVDF Polyvinylidene fluoride Electrical and thermal insulating products with food slipping propertiesChemically inertInformation provided by Isoflon. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 933-2 Moisture Resistant Chip Encapsulant TRA-BOND 933-2 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical.. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
CTE, linear | 120 µm/m-°C @Temperature -40.0 - 140 °C |
66.7 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
BLUESTAR BS025 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
BLUESTAR BS270 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 120 - 140 µm/m-°C @Temperature 20.0 °C |
66.7 - 77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CP - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTRODAL TF Polyoxymethylene + PTFE This material is high strength and high heat strength dimensional stability. Applications include racks and annular gears, dimensionally accurate structural components for pumps, and housings and t.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |