Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792, ISO 1183 |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific) Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available .. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds RKT 736/K1 Rigid PVC, Extrusion Lead Free Transparent profiles |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Multibase Multi-Flamâ„¢ 205 HFRI Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP LX04015 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LX04015 is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include: Electrically Conductive |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PA6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Conductive and LubricatedAppearance: BlackInform.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant, Halogen Free and Impact ModifiedAppearance: BlackI.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GFT1675-N1 33% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 519 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® BGK-30 X PA6-(GF+GB)30 Information provided by EMS Grivory |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 55580R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for th.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | Side 2 Silicone Property; Arlon SQA-TMS-024 |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | cured; ASTM D794 |
3M Scotchcast™ 262 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 262 is a widely used, well-known general purpose epoxy powder resin. A one-part, red pigmented, rapid heat-curing product, it is designed to provide a continuous, toug.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | Layer 1, Silicone Property; Arlon SQA-TMS-024 |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66
(Unverified Data**) Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | (Dry) |
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |