Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CA - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
PTS POM-25 Acetal Copolymer Information provided by PTS LLC. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
PTS POM-90 Acetal Copolymer Information provided by PTS LLC. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 120 - 140 µm/m-°C @Temperature 20.0 °C |
66.7 - 77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
CTE, linear | 120 - 140 µm/m-°C | 66.7 - 77.8 µin/in-°F | Average value: 126 µm/m-°C Grade Count:16 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PVDF Polyvinylidene Fluoride Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
CTE, linear | 120 - 130 µm/m-°C | 66.7 - 72.2 µin/in-°F | ASTM D696 |
Guarniflon PTFE G400 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM E831 |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | 25°C to 100°C; ASTM D696 |
Guarniflon MFA Fluoropolymer It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It .. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 - 100 °C |
66.7 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon PTFE Polytetrafluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 120 - 140 µm/m-°C @Temperature 20.0 °C |
66.7 - 77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Zeus PFA Tubing PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar.. |
|||
CTE, linear | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
BLUESTAR BS130 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
ExxonMobil Paxon™ BC50-100 Sheet Extrusion and Blow Molding Resin
(discontinued **) BC50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Information provided by ExxonMobil .. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
CTE, linear | 120 - 140 µm/m-°C @Temperature 20.0 °C |
66.7 - 77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
CTE, linear | 120 - 216 µm/m-°C | 66.7 - 120 µin/in-°F | Average value: 161 µm/m-°C Grade Count:12 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
PTS POM-270 Acetal Copolymer Information provided by PTS LLC. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 - 100 °C |
66.7 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | Above Tg |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
CTE, linear | 120 - 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 - 66.7 µin/in-°F @Temperature 212 - 392 °F |
Average value: 120 µm/m-°C Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |