Polymer Property : Mold Temperature = 177 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 135 - 177 °C
275 - 350 °F
Oxford Polymers PPS-30GF-10PTFE-BK PPS, 30% Glass Fiber Reinforced, 10% PTFE
Product Description: Glass Fiber (30% Reinforced), 10% PTFE, Polyphenylene sulfide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAppearance: BlackInformation pr..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1399 X 102903 J Polyphenylene Sulfide (PPS) Thermally Conductive - Electrically Insulative  (d
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1300 AR 15 SI 2  Polyphenylene Sulfide (PPS) Aramid Fiber 15% - Silicone 2%  
Aramid Fiber 15% - Silicone 2%Comments:Aramid FiberSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informatio..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company EMI 1360.7  Polyphenylene Sulfide (PPS) Shielding - Stainless Steel Fiber 7%  (d
Shielding - Stainless Steel Fiber 7%Comments:EMI/RFI ShieldingESD ProtectionStainless Steel FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company ESD C 2280  Polyetheretherketone (PEEK) Conductive - Carbon Fiber  (discontinued
Conductive - Carbon FiberComments:ConductiveESD ProtectionCarbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informatio..
Mold Temperature 149 - 177 °C
300 - 351 °F
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 AR 10  Polyetherimide (PEI) Aramid Fiber 10%  (discontinued **)
Aramid Fiber 10%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%  (disc
Shielding - Nickel-Coated Carbon Fiber 20%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pig..
Mold Temperature 51.7 - 177 °C
125 - 350 °F
Average value: 151 °C Grade Count:38
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Mold Temperature 149 - 177 °C
300 - 351 °F
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Mold Temperature 149 - 177 °C
300 - 351 °F
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company ESD A 2180 Polyetherimide (PEI), Carbon Fiber - ESD Protection - Static Dissipative
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1300 D TFE 20 Polyphenylene Sulfide (PPS), PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1300 TC-C-30 Polyphenylene Sulfide (PPS), Thermally Conductive - Electrically Conductive - Flame Retardant
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1303 D Polyphenylene Sulfide (PPS), Glass Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1379 Polyphenylene Sulfide (PPS), Glass Fiber - Mineral
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1382 AR 10 TFE 15 Polyphenylene Sulfide (PPS) Carbon Fiber - Aramid Fiber - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1400 AG-330 Polyethersulfone (PES), Glass Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2184 HEC Polyetherimide (PEI), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2187 Polyetherimide (PEI); Carbon Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2199 X 130019 A Polyetherimide (PEI); Carbon Fiber - Static Dissipative - (Preliminary Data Sheet)
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company ESD 1382 TFE 15 Polyphenylene Sulfide (PPS) Carbon Fiber - PTFE Lubricated - ESD Protection
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1387 P-1 Polyphenylene Sulfide (PPS), Carbon Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1399 X 115071 F Polyphenylene Sulfide (PPS), Glass Fiber - Carbon Nanotube - Electrically Conductive
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1481 N TFE 15 Polyethersulfone (PES), Carbon Fiber - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 351 °F
Celanese CoolPoly® E5105 Thermally Conductive Polyphenylene Sulfide
CoolPoly E series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows ..
Mold Temperature 149 - 177 °C
300 - 350 °F
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester
BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1381 HEC  Polyphenylene Sulfide (PPS) Nickel-Coated Carbon Fiber 10% - EMI/ESD &n
Nickel-Coated Carbon Fiber 10% - EMI/ESDComments:EMI/RFI/ESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1405 HF TFE 15  Polyethersulfone (PES) Glass Fiber 30% - PTFE 15% - High Flow &nb
Glass Fiber 30% - PTFE 15% - High FlowComments:Glass FiberPTFE LubricatedHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect propertie..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1399 X 127548 A Polyphenylene Sulfide (PPS); Glass Fiber - Carbon Fiber - ESD Protection
This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.
Copyright © lookpolymers.com All Rights Reserved