Polymer Property : Injection Pressure = 34.5 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 34.5 - 82.7 MPa
5000 - 12000 psi
RTP Company RTP 3485-1 Liquid Crystal Polymer (LCP), Carbon Fiber
Injection Pressure 34.5 - 103 MPa
5000 - 15000 psi
Average value: 80.4 MPa Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Injection Pressure 34.5 - 150 MPa
5000 - 21800 psi
Average value: 119 MPa Grade Count:4
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Average value: 89.1 MPa Grade Count:3
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Injection Pressure 34.5 - 172 MPa
5000 - 25000 psi
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc.
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated
Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® NY1599-N Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2700 S-30A Saturated Styrenic Block Copolymer, General Purpose
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2700 S-80A Z Saturated Styrenic Block Copolymer (TES/SEBS or other), FDA Compliant Ingredients
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2740 S-30A Saturated Styrenic Block Copolymer, General Purpose
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2740 S-50A Saturated Styrenic Block Copolymer, General Purpose
Injection Pressure 34.5 - 207 MPa
5000 - 30000 psi
Denka STYROL MW1 Polystyrene
"DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," ..
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled
Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistanc..
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2800 B-55A UV Thermoplastic Polyolefin Elastomer (TEO), UV Stabilized  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Injection Pressure 34.5 - 103 MPa
5000 - 15000 psi
LookPolymers® 1140 E7 Polyphenylene Sulfide (PPS)
Description: Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grad..
Injection Pressure 34.5 - 82.7 MPa
5000 - 12000 psi
RTP Company RTP 3405-1 Liquid Crystal Polymer (LCP), Glass Fiber
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2800 B-80A Z Thermoplastic Polyolefin Elastomer, FDA Compliant Ingredients  (discontinued **)&
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2740 S-45A Saturated Styrenic Block Copolymer (TES/SEBS or other)  (discontinued **)
Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
RTP Company RTP 2700 S-80A Saturated Styrenic Block Copolymer, General Purpose