Polymer Property : Electrical Resistivity = 1.00e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ISO data
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
RTP Company RTP 1300 C AR 35  Polyphenylene Sulfide (PPS) Aramid Fiber 35%  (discontinued **
Aramid Fiber 35%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
Average value: 2.90e+15 ohm-cm Grade Count:10
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)  (discontinued **)
ENSILON 6/6 GF30 is a 30% glass-fiber-reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection, and superior abrasion..
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
Average value: 8.71e+15 ohm-cm Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Electrical Resistivity 1.00e+15 - 2.00e+16 ohm-cm
1.00e+15 - 2.00e+16 ohm-cm
Average value: 1.01e+16 ohm-cm Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 2426 F LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 3040 D LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Ineos ABS Lustran® H606 LS
Improved heat and UV resistance.,Property data per ISO test methods.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 1852 H SW 413 LDPE
Blow moldings, injection moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Momentive Performance Materials RTV6136 Potting/Encapsulating Gel
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 1812 E LDPE
Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH50
Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Covestro Bayblend® R-T 60 Polycarbonate/ABS Blend
Recycled grade in which carefully reclaimed old parts and production rejects and/or scrap from all processes of manufacturing or processing undergo material recycling. Slightly decreased impact stre..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Covestro Bayblend® T 84 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Evonik Corporation Vestoran® X7342 beige PPE
Uses: Housings, automobile industry, electrical industry.ISO data as provided by the manufacturer.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Covestro Makrolon® 1143 Polycarbonate
Pseudoplastic behavior and high viscosity extrusion grade with UV stabilizer and easy mold release, special grade for twin-wall sheet.Information provided by Bayer.As of 1 September 2015, Bayer Mate..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned)
Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Arkema Group Orgalloy® RS 6620 Nylon 66 Alloy, 20% Glass Fiber (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry)
Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade
Injection moldingsData was collected by ISO methods and provided by BASF.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BASF Polystyrol® 144 C Polystyrene (Europe)
Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF.
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced
A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Ceradyne Ceralloy® 1370DP Aluminum Nitride
Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Arkema Group Orgalloy® RS 6000CD Nylon 6 Alloy, Rigid Grade (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ISO data
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Average value: 1.00e+15 ohm-cm Grade Count:5
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
3M Dyneon™ Aflas® FA-150P PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..