Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 5.00 - 7.00 kJ/m² @Temperature -40.0 - -30.0 °C |
2.38 - 3.33 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 5.88 kJ/m² Grade Count:16 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 7.00 kJ/m² | 1.43 - 3.33 ft-lb/in² | Average value: 5.14 kJ/m² Grade Count:9 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 7.00 kJ/m² | 2.38 - 3.33 ft-lb/in² | Average value: 5.75 kJ/m² Grade Count:4 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -40.0 - -40.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 13.1 kJ/m² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Thickness 4.00 - 4.00 mm |
3.33 - 3.33 ft-lb/in² @Thickness 0.157 - 0.157 in |
Average value: 13.1 kJ/m² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 4.00 - 7.00 kJ/m² | 1.90 - 3.33 ft-lb/in² | Average value: 5.00 kJ/m² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 7.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.952 - 3.33 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.71 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 7.00 kJ/m² @Temperature -40.0 - -20.0 °C |
2.86 - 3.33 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 6.50 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Notched (ISO) | 0.700 - 7.00 kJ/m² @Temperature -40.0 - -30.0 °C |
0.333 - 3.33 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.58 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Notched (ISO) | 3.50 - 7.00 kJ/m² | 1.67 - 3.33 ft-lb/in² | Average value: 4.79 kJ/m² Grade Count:14 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 3.00 - 7.00 kJ/m² | 1.43 - 3.33 ft-lb/in² | Average value: 4.65 kJ/m² Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 7.00 kJ/m² | 1.90 - 3.33 ft-lb/in² | Average value: 5.33 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |