Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
RTP Company RTP 4001 TFE 15 SI 2  Polyphthalamide (PPA) Glass Fiber 10% - PTFE 15% - Silicone 2% &
Glass Fiber 10% - PTFE 15% - Silicone 2%Comments:Glass FiberPTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affe..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Polycasa Acryl® G 88 E Acrylic
Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs ..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Polimeri Europa KOBLEND PCA 839F PC+ABS  (discontinued **)
Symbol according to ISO 1043/1: PC+ABSUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses...
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend  (discontinued **)
Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
RTP Company RTP 205D HS TFE 15  Nylon 6/12 (PA 6/12) Glass Fiber 30% - PTFE 15% - Heat Stable &nb
Glass Fiber 30% - PTFE 15% - Heat StableComments:Glass FiberPTFE LubricatedHeat StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect p..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 3226 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade
Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade
Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BN Component
Momentive Performance Materials FPC APC Boron Nitride (BN)/Al2O3 Water Based Coating
Solids content > 25%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Momentive Performance Materials HBR Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 1852 H SW 413 LDPE
Blow moldings, injection moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Evonik Corporation Vestamid® L1901 nf (dry properties) Nylon 12
ISO data as provided by the manufacturer.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Evonik Corporation Vestamid® L2140B nf (dry properties) Nylon 12
Uses: Tubing and profiles for food contact applications.ISO data as provided by the manufacturer.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Evonik Corporation Vestoran® 1900 nf PPE
Filler-free, amorphous PPE resin.Applications: Machinery, plastic & rubber composite technology.ISO data as provided by the manufacturer.
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET
30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Arkema Group Orgalloy® RS 6020 Nylon 6 Alloy, 20% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties...
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced
Glass fiber reinforced grade containing halogen-free flame-retardant; for moldings with high heat resistance and stiffness (e.g. relay parts, controller and switch housings).Data was collected by IS..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BASF Novolen® 3225 MC Polypropylene
Grade containing slip and blocking agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BASF Novolen® 3240 NC Polypropylene
Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
BASF Novolen® 3325 MC Polypropylene
Grade containing slip and blocking agents, for cast film.Data was collected by ISO methods and provided by BASF.
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Ashley Polymers Ashlene® RH190-PF Acetal, PTFE Filled
A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
CENTROPLAST CENTROLEN PE-HD Polyethylene high density
This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ISO data
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant nylon 6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retard..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ISO data
BASF Capron® HPN 9233G HS BK-102 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced nylon 6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times ..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cm
1.00e+15 - 1.00e+17 ohm-cm
Average value: 2.74e+16 ohm-cm Grade Count:14
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
LyondellBasell Lupolen® 1800 H LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.