Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 - 0.801 J/cm | 0.300 - 1.50 ft-lb/in | Average value: 0.349 J/cm Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.534 - 0.801 J/cm | 1.00 - 1.50 ft-lb/in | Average value: 0.596 J/cm Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.526 J/cm Grade Count:32 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Izod Impact, Notched | 0.320 - 0.801 J/cm | 0.599 - 1.50 ft-lb/in | Average value: 0.575 J/cm Grade Count:26 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Izod Impact, Notched | 0.374 - 0.801 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.587 J/cm Grade Count:12 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.534 - 0.801 J/cm | 1.00 - 1.50 ft-lb/in | Average value: 0.661 J/cm Grade Count:21 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.320 - 0.801 J/cm | 0.600 - 1.50 ft-lb/in | Average value: 0.564 J/cm Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Izod Impact, Notched | 0.374 - 0.801 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.605 J/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Izod Impact, Notched | 0.534 - 0.801 J/cm | 1.00 - 1.50 ft-lb/in | Average value: 0.601 J/cm Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.617 J/cm Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.497 J/cm Grade Count:5 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.400 - 0.801 J/cm | 0.749 - 1.50 ft-lb/in | Average value: 0.586 J/cm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.320 - 0.801 J/cm | 0.600 - 1.50 ft-lb/in | Average value: 0.686 J/cm Grade Count:7 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.374 - 0.801 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.618 J/cm Grade Count:8 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 0.534 - 0.801 J/cm @Temperature 22.8 °C |
1.00 - 1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.737 - 0.801 J/cm | 1.38 - 1.50 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |
|||
Izod Impact, Notched | 0.400 - 0.801 J/cm | 0.750 - 1.50 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Izod Impact, Notched | 0.587 - 0.801 J/cm | 1.10 - 1.50 ft-lb/in | ASTM D256 |
Aaron Industries AVPS M 100-2 Virgin Polystyrene Melt flow index may be specified. |
|||
Izod Impact, Notched | 0.641 - 0.801 J/cm | 1.20 - 1.50 ft-lb/in | ASTM D256 |
Aaron Industries AAROLENE® ARPS MI 100-2 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Izod Impact, Notched | 0.481 - 0.801 J/cm | 0.900 - 1.50 ft-lb/in | Average value: 0.596 J/cm Grade Count:24 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.493 J/cm Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.498 J/cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Izod Impact, Notched | 0.220 - 0.801 J/cm | 0.412 - 1.50 ft-lb/in | Average value: 0.471 J/cm Grade Count:18 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |