Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | ISO 179 |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 - 2.80 J/cm² @Temperature -30.0 - -30.0 °C |
13.3 - 13.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.80 J/cm² Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1850-7784 PBT, with glass fiber, glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-8076 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG10-BN00N1 Nylon 6 10% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6 Applications: Mid-Grade CBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | |
BASF Polystyrol® 168 N Polystyrene (Europe) High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 2.80 - 5.00 J/cm² | 13.3 - 23.8 ft-lb/in² | Average value: 4.14 J/cm² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² | 13.3 - 25.2 ft-lb/in² | Average value: 4.40 J/cm² Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² @Temperature -30.0 - -20.0 °C |
13.3 - 25.2 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.68 J/cm² Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |