Polymer Property : Thermal Conductivity = 0.300 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.167 - 0.300 W/m-K
1.16 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.292 W/m-K Grade Count:16
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Thermal Conductivity 0.110 - 0.300 W/m-K
0.763 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.182 W/m-K Grade Count:62
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Thermal Conductivity 0.290 - 0.300 W/m-K
2.01 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.296 W/m-K Grade Count:7
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Thermal Conductivity 0.255 - 0.300 W/m-K
1.77 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.287 W/m-K Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Thermal Conductivity 0.167 - 0.300 W/m-K
1.16 - 2.08 BTU-in/hr-ft²-°F
ASTM C177
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..
Thermal Conductivity 0.250 - 0.300 W/m-K
1.74 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.262 W/m-K Grade Count:9
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Thermal Conductivity 0.200 - 0.300 W/m-K
1.39 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.235 W/m-K Grade Count:40
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..