Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 280 °C | 536 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hFR31 PPS / AR Polyphenylene Sulfide Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hMR60 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hMR60DL Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | |
Williams Advanced Alloys WS280B Solder (Au80/Sn20) All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy E-16901B PPS Alloy, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 285 °C | 536 - 545 °F | Average value: 282 °C Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |