Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 66, Glass Reinforced, Impact Grade

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 66, Glass Reinforced, Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.12 - 1.60 g/cc
0.0405 - 0.0578 lb/in³
Average value: 1.29 g/cc Grade Count:122
Filler Content 5.00 - 50.0 %
5.00 - 50.0 %
Average value: 23.3 % Grade Count:34
Water Absorption 0.300 - 6.40 %
0.300 - 6.40 %
Average value: 0.937 % Grade Count:71
Moisture Absorption at Equilibrium 0.450 - 2.70 %
0.450 - 2.70 %
Average value: 1.69 % Grade Count:20
Water Absorption at Saturation 4.50 - 6.50 %
4.50 - 6.50 %
Average value: 5.70 % Grade Count:5
Linear Mold Shrinkage 0.000600 - 0.0160 cm/cm
0.000600 - 0.0160 in/in
Average value: 0.00542 cm/cm Grade Count:110
Linear Mold Shrinkage, Transverse 0.00700 - 0.0130 cm/cm
0.00700 - 0.0130 in/in
Average value: 0.00929 cm/cm Grade Count:14
Ash 33.0 - 33.0 %

@Temperature 650 - 650 °C
33.0 - 33.0 %

@Temperature 1200 - 1200 °F
Average value: 33.0 % Grade Count:1
Mechanical Properties Metric English Comments
Hardness, Rockwell M 76.0 - 95.0
76.0 - 95.0
Average value: 87.1 Grade Count:14
Hardness, Rockwell R 98.0 - 122
98.0 - 122
Average value: 115 Grade Count:63
Tensile Strength, Ultimate 58.6 - 221 MPa
8500 - 32100 psi
Average value: 116 MPa Grade Count:81
Tensile Strength, Yield 46.9 - 159 MPa
6800 - 23000 psi
Average value: 116 MPa Grade Count:41
Elongation at Break 2.00 - 12.0 %
2.00 - 12.0 %
Average value: 4.27 % Grade Count:117
Elongation at Yield 3.00 - 6.00 %
3.00 - 6.00 %
Average value: 3.85 % Grade Count:4
Modulus of Elasticity 2.76 - 15.2 GPa
400 - 2200 ksi
Average value: 6.95 GPa Grade Count:59
Flexural Yield Strength 16.0 - 360 MPa
2320 - 52200 psi
Average value: 166 MPa Grade Count:97
Flexural Modulus 2.07 - 36.2 GPa
300 - 5250 ksi
Average value: 6.17 GPa Grade Count:106
Compressive Yield Strength 28.0 - 179 MPa
4060 - 26000 psi
Average value: 120 MPa Grade Count:22
Izod Impact, Notched 0.374 - 6.51 J/cm
0.700 - 12.2 ft-lb/in
Average value: 1.65 J/cm Grade Count:92
1.0678 - 1.0678 J/cm

@Temperature -40.0 - -40.0 °C
2.0004 - 2.0004 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.07 J/cm Grade Count:9
1.0678 - 1.0678 J/cm

@Thickness 3.17 - 3.17 mm
2.0004 - 2.0004 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.07 J/cm Grade Count:9
Izod Impact, Unnotched 4.64 - 5340 J/cm
8.69 - 10000 ft-lb/in
Average value: 8.60 J/cm Grade Count:47
Izod Impact, Notched (ISO) 2.94 - 30.0 kJ/m²
1.40 - 14.3 ft-lb/in²
Average value: 15.1 kJ/m² Grade Count:17
6.00 - 19.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.86 - 9.04 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 11.6 kJ/m² Grade Count:11
Izod Impact, Unnotched (ISO) 50.0 - 90.0 kJ/m²
23.8 - 42.8 ft-lb/in²
Average value: 79.3 kJ/m² Grade Count:7
50.0 - 95.0 kJ/m²

@Temperature -30.0 - -30.0 °C
23.8 - 45.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 75.8 kJ/m² Grade Count:6
Charpy Impact Unnotched 3.50 - 10.5 J/cm²
16.7 - 50.0 ft-lb/in²
Average value: 7.54 J/cm² Grade Count:18
3.50 - 8.70 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 41.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.29 J/cm² Grade Count:9
Charpy Impact, Notched 0.600 - 4.00 J/cm²
2.86 - 19.0 ft-lb/in²
Average value: 2.15 J/cm² Grade Count:21
0.500 - 1.80 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 8.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.10 J/cm² Grade Count:11
Thermal Properties Metric English Comments
CTE, linear 13.0 - 400 µm/m-°C
7.22 - 222 µin/in-°F
Average value: 60.2 µm/m-°C Grade Count:46
CTE, linear, Transverse to Flow 78.0 - 130 µm/m-°C
43.3 - 72.2 µin/in-°F
Average value: 103 µm/m-°C Grade Count:3
Thermal Conductivity 0.300 - 0.504 W/m-K
2.08 - 3.50 BTU-in/hr-ft²-°F
Average value: 0.422 W/m-K Grade Count:11
Melting Point 252 - 275 °C
486 - 527 °F
Average value: 258 °C Grade Count:50
Maximum Service Temperature, Air 110 - 250 °C
230 - 482 °F
Average value: 160 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 210 - 304 °C
410 - 580 °F
Average value: 248 °C Grade Count:90
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 252 °C
167 - 486 °F
Average value: 228 °C Grade Count:110
Vicat Softening Point 228 - 250 °C
442 - 482 °F
Average value: 237 °C Grade Count:12
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:80
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 1.00e+15 ohm-cm
10.0 - 1.00e+15 ohm-cm
Average value: 2.03e+14 ohm-cm Grade Count:66
Surface Resistance 1.00e+6 - 1.00e+15 ohm
1.00e+6 - 1.00e+15 ohm
Average value: 4.05e+13 ohm Grade Count:30
Dielectric Constant 3.50 - 6.90
3.50 - 6.90
Average value: 4.22 Grade Count:19
Dielectric Strength 11.8 - 90.0 kV/mm
300 - 2290 kV/in
Average value: 24.1 kV/mm Grade Count:46
Dissipation Factor 0.0130 - 0.0200
0.0130 - 0.0200
Average value: 0.0152 Grade Count:10
Dielectric Loss Index 0.0120 - 0.190
0.0120 - 0.190
Average value: 0.0751 Grade Count:7
Arc Resistance 82.0 - 90.0 sec
82.0 - 90.0 sec
Average value: 85.8 sec Grade Count:8
Comparative Tracking Index 350 - 600 V
350 - 600 V
Average value: 522 V Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 270 - 300 °C
518 - 572 °F
Average value: 285 °C Grade Count:38
Nozzle Temperature 250 - 304 °C
482 - 580 °F
Average value: 283 °C Grade Count:4
Melt Temperature 260 - 310 °C
500 - 590 °F
Average value: 282 °C Grade Count:23
Mold Temperature 50.0 - 110 °C
122 - 230 °F
Average value: 84.9 °C Grade Count:55
Drying Temperature 73.9 - 100 °C
165 - 212 °F
Average value: 81.3 °C Grade Count:17
Moisture Content 0.180 - 1.60 %
0.180 - 1.60 %
Average value: 0.291 % Grade Count:15
Injection Pressure 4.96 - 124 MPa
720 - 18000 psi
Average value: 93.5 MPa Grade Count:34
Users viewing this material also viewed the following: