Polymer Property : Izod Impact, Notched (ISO) = 19.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.30 - 19.0 kJ/m²
0.619 - 9.04 ft-lb/in²
Average value: 3.13 kJ/m² Grade Count:23
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 12.0 - 19.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.71 - 9.04 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 15.5 kJ/m² Grade Count:2
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Izod Impact, Notched (ISO) 5.00 - 19.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.38 - 9.04 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 10.2 kJ/m² Grade Count:111
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Notched (ISO) 6.00 - 19.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.86 - 9.04 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 11.6 kJ/m² Grade Count:11
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Copyright © lookpolymers.com All Rights Reserved