Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 260 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
Plastcom SLOVAMID 66 MI LS PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Melt Temperature 260 - 280 °C
500 - 536 °F
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre
FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melt Temperature 260 - 277 °C
500 - 531 °F
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Melt Temperature 260 - 282 °C
500 - 540 °F
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM)
Information provided by Ravago.
Melt Temperature 260 - 270 °C
500 - 518 °F
DuPont Performance Polymers Crastin® SK609 BK851 PBT  (Unverified Data**)
Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Melt Temperature 260 °C
500 °F
Injection molding; ISO 294
Celanese Celanex® 3316 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Melt Temperature 260 - 280 °C
500 - 536 °F
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Melt Temperature 260 - 280 °C
500 - 536 °F
DAM; Injection Molding
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Melt Temperature 260 - 300 °C
500 - 572 °F
Average value: 275 °C Grade Count:6
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Melt Temperature 260 - 270 °C
500 - 518 °F
Cast Film
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an..
Melt Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Melt Temperature 260 - 280 °C
500 - 536 °F
Injection Molding
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
Melt Temperature 260 - 290 °C
500 - 554 °F
Recommended
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers
PA 6-Copolymer, 15% glass fibers, injection molding, impact modified
Melt Temperature 260 - 270 °C
500 - 518 °F
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS.
Melt Temperature 260 - 280 °C
500 - 536 °F
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber
PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS.
Melt Temperature 260 - 280 °C
500 - 536 °F
ISO 294
Gromax BFG10-BN00N1 Nylon 6 10% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Melt Temperature 260 °C
500 °F
for test specimens; ISO 294
Lanxess Pocan® B 1701 000000 PBT
PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS.
Melt Temperature 260 °C
500 °F
Injection Molding; ISO 294
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Melt Temperature 260 - 279 °C
500 - 535 °F
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
Melt Temperature 260 - 277 °C
500 - 531 °F
Styron EMERGEâ„¢ 4310-22 Polycarbonate
EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn..
Melt Temperature 260 - 280 °C
500 - 536 °F
Supreme Petrochem SP 6456 High Heat Polystyrene
Characteristics High heat resistance & strength Very good flow properties Available in any dark colorsProcessing Injection moldingApplications Instrument enclosures TV components Electrical encl..
Melt Temperature 260 - 290 °C
500 - 554 °F
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber
SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers
Melt Temperature 260 °C
500 °F
Injection Molding; ISO 294
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c..
Melt Temperature <= 260 °C
<= 500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Melt Temperature <= 260 °C
<= 500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Melt Temperature 260 °C
500 °F
Injection molding
BASF Ultramid® 8202C PA6 (Conditioned)
Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique ..
Melt Temperature 260 - 290 °C
500 - 554 °F
CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melt Temperature 260 °C
500 °F
for shrinkage test, Optimal
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
Melt Temperature 260 - 280 °C
500 - 536 °F
Injection Molding
Styrolution Luran® S KR 2867 C WU Colored ASA+PC
Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO..
Melt Temperature 260 - 277 °C
500 - 531 °F
PolyOne Edgetek® XT XT-500-CX00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Copyright © lookpolymers.com All Rights Reserved