Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 350 V | 350 V | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Comparative Tracking Index | >= 350 V | >= 350 V | IEC 60112 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Cond)
(discontinue The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Lanxess Pocan® B 3225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Comparative Tracking Index | 350 V | 350 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Comparative Tracking Index | 350 V | 350 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding... |
|||
Comparative Tracking Index | 350 V | 350 V | TS EN 60112 |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Comparative Tracking Index | 350 V | 350 V | GB/4207 |
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6 Applications: Mid-Grade CBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content |
|||
Comparative Tracking Index | 350 V | 350 V | |
Covestro Bayblend® KU 2-1500 Polycarbonate/ABS Blend Flame retardant extrusion grade.Applications: Bulky parts for DT-copying machines.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and official.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Covestro Bayblend® KU 2-1514* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeball indentation temperature =125 °CVicat/B 120 temperature = 136 °CUL-listing 94 V-0 at 1.5 mmsuitable for supporting life componen.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
DSM Stanyl® 46HF5040 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Comparative Tracking Index | 350 V | 350 V | dry; IEC 60112 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 350 V | 350 V | Test Solution A; IEC 112 |
BASF Ultradur B 4300 G6 High Speed Unc. 30% Glass Filled PBT Ultradur B 4300 G6 High Speed Unc. is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Comparative Tracking Index | 350 V | 350 V | Test solution A; IEC 60112 |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Conditioned) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Comparative Tracking Index | 350 V | 350 V | Test solution A; IEC 60112 |
BASF Ultramid® C3U10 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Comparative Tracking Index | 350 V | 350 V | |
Radici Radiflam® S AE (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Comparative Tracking Index | >= 350 V | >= 350 V | IEC 60112 |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |