Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180/1U |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180/1U |
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
(discontinued **) Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Qualchem Danamid FGFHUV-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial light.Information provided by Qualchem Zrt. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 82.0 kJ/m² | 23.8 - 39.0 ft-lb/in² | Average value: 62.7 kJ/m² Grade Count:7 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180-1U |
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP PDX-U-05314 PPA (Asia Pacific) LNP* Lubricomp* PDX-U-05314 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON PX93058 PA 6 (Europe-Africa-Middle East) LNP*STATKON*PX93058 is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF007ESS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF007ESS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UF007SXC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007SXC is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include : Heat Stabilized . |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RKN14 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RKN14 is a compound based on Nylon 66 resin containing Mineral, MOS2. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East) LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Tipco Tipcofil® AGM 602 - 10% Mineral & 20% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Mineral + 20% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA66 30Y D61 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT 403 M-G20 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G15 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-MFC-G20 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
BLUESTAR 403HF-G20 PBT, 20% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1U |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |