Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Protective Coating PC-Plumbing Epoxy Putty™ Hand Moldable, Multi-Purpose Epoxy Putty Stick Description: After Mixing, PC-Plumbing™ can be used to repair split and leaking pipes, tanks, drums, castings, ducts, valves and tools. It can be used wherever metal is missing, dented, broken, or .. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Dielectric Strength | 11.8 - 21.7 kV/mm | 300 - 550 kV/in | Average value: 16.3 kV/mm Grade Count:24 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 11.8 - 48.2 kV/mm | 300 - 1220 kV/in | Average value: 17.0 kV/mm Grade Count:103 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; 1/8 inch; ASTM D149 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Dielectric Strength | 11.8 - 120 kV/mm | 300 - 3050 kV/in | Average value: 34.3 kV/mm Grade Count:109 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Plenco 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
IDI Composites 46-12 Thermoset Polyester, Molding Highest strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black Information provided by ITW Devcon |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 3.00 mm |
300 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Step by Step; ASTM D149 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm @Thickness 3.17 mm |
300 - 400 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7650-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D1000 |
3M Scotch™ 2210 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm | 300 - 400 kV/in | |
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Dielectric Strength | 11.8 - 45.0 kV/mm | 300 - 1140 kV/in | Average value: 25.8 kV/mm Grade Count:12 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; 1/8 inch; ASTM D149 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |