Injection Pressure 75.8 - 124 MPa
11000 - 18000 psi
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 4007 TFE 10 Polyphthalamide (PPA), Glass Fiber - PTFE Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 4009 Polyphthalamide (PPA), Glass Fiber
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 208 K Polyarylamide (PAA), Glass Fiber  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2105 HF  Polyetherimide (PEI) Glass Fiber 30% - High Flow  (discontinued **)
Glass Fiber 30% - High FlowComments:Glass FiberHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by ..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 209D HS  Nylon 6/12 (PA 6/12) Glass Fiber 50% - Heat Stable  (discontinued *
Glass Fiber 50% - Heat StableComments:Glass FiberHeat StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 207D HS UV  Nylon 6/12 (PA 6/12) Glass Fiber 40% - Heat Stable - UV Stable  
Glass Fiber 40% - Heat Stable - UV StableComments:Glass FiberHeat StabilizedUV StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect pr..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 200 D AR 10 TFE 15 Nylon 6/12 (PA), Aramid Fiber - PTFE Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 200 GB 20 Z Nylon 6/6 (PA) Glass Bead - FDA Compliant Ingredients
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 201 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 202 TFE 13 SI 2 Nylon 6/6 (PA) Glass Fiber - PTFE Lubricated - Silicone Lubricated
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2183 HF Polyetherimide (PEI), Carbon Fiber
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2187 Polyetherimide (PEI); Carbon Fiber
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2200 HF TFE 15 Polyetheretherketone (PEEK), PTFE Lubricated - High Flow
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 283 HS Nylon 6/6 (PA), Carbon Fiber - Heat Stabilized
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 1385 D TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 200 TC-C-29 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2200 HF TFE 5 Polyetheretherketone (PEEK), PTFE Lubricated - High Flow
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 299 X 93636 B Nylon 6/6 (PA), Wear Resistant
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 200D AR 10  Nylon 6/12 (PA 6/12) Aramid Fiber 10%  (discontinued **)
Aramid Fiber 10%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2800B-40D HF  Thermoplastic Vulcanizate Elastomer (TPV) 40 Shore D - High Flow &n
40 Shore D - High FlowComments:40-D DurometerHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT..
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2299 X 113763 B Polyetheretherketone (PEEK), Carbon Fiber - Aramid Fiber - PTFE Lubricated - Perfluoropolyether Oil
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 905 TFE 15 Polysulfone (PSU), Glass Fiber - PTFE Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 203B TFE 15  Nylon 6/10 (PA 6/10) Glass Fiber 20% - PTFE 15%  (discontinued
Glass Fiber 20% - PTFE 15%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company ESD C 2800-65A ESD Protection - Electrically Conductive, ESD Protection - Electrically Conductive  
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 4000 TFE 18 SI 2  Polyphthalamide (PPA) PTFE 18% - Silicone 2%  (discontinue
PTFE 18% - Silicone 2%Comments:PTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pro..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 4099 X 68912 A  Polyphthalamide (PPA) Long Glass Fiber 40% - Heat Stable  (d
Long Glass Fiber 40% - Heat StableComments:Long Glass FiberHeat StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Inform..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 225 Nylon 6/6 (PA), Mineral
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
RTP Company RTP 2299 X 115070 F Polyetheretherketone (PEEK) Carbon Nanotube - Electrically Conductive - Permanently Static Dissipative