Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 16.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 16.0 MPa
2320 psi
ASTM D790
NYCOA 7551 Copolymer Nylon Alloy
resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc.
Flexural Yield Strength 16.0 - 54.0 MPa
2320 - 7830 psi
Average value: 36.5 MPa Grade Count:47
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Flexural Yield Strength 16.0 - 360 MPa
2320 - 52200 psi
Average value: 166 MPa Grade Count:97
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Flexural Yield Strength 16.0 MPa
2320 psi
at 3.5%
Biomer P209 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Flexural Yield Strength 16.0 - 200 MPa
2320 - 29000 psi
Average value: 82.1 MPa Grade Count:285
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..