LyondellBasell Petrothene® NA952000 Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA952000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of processability, toughness and drawdown. Regulatory StatusThe NA 952 basic resin meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 952 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 6"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
2:1 BUR; 25 mil die gap
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.4 MPa
1800 psi
Molded; ASTM D638
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Elongation at Break 650 %
650 %
Molded; ASTM D638
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
Dart Drop Test 110 g
0.243 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
Film Tensile Strength at Break, TD 15.9 MPa
2300 psi
ASTM D882
1% Secant Modulus, MD 183 MPa
26500 psi
ASTM D882
1% Secant Modulus, TD 221 MPa
32000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Descriptive Properties Value Comments
Antiblock None
Slip None