Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Nylene® PA6/6 Impact Modified 311 HS Nylon 6/6 Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Nylene® PA6/6 Impact Modified 4120 HS Nylon 6/6; MoS2 lube High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Melting Point | 252 °C | 486 °F | ASTM D789 |
PTS Trimid® N66-T100 Toughened Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | <= 252 °C | <= 486 °F | DSC test |
Invista 2202 Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Melting Point | <= 252 °C | <= 486 °F | DSC |
Indorama Auriga Polymers Polyclear™ Refresh 1101 PET Resin Description: Polyclear® Refresh PET 1101 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Refresh PET 1101 has excellent clarity a.. |
|||
Melting Point | 252 - 295 °C | 486 - 563 °F | |
Williams Advanced Alloys WS295 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | <= 252 °C | <= 486 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope.. |
|||
Melting Point | <= 252 °C | <= 486 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Melting Point | 252 °C | 486 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 525-33G Nylon 66, 33% Glass Reinforced High impact Nylon 66 reinforced with 33% glass fibers, lubricated.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 525LD-33G Nylon 66, 33% Glass Reinforced High impact Nylon 66 reinforced with 33% glass fibers, lubricated.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 527-13G Nylon 66, 13% Glass Reinforced A 13% glass reinforced, impact modified Nylon 66.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 527-25G Nylon 66, 25% Glass Reinforced A 25% glass reinforced impact modified Nylon 66.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced A high impact nylon with 14% glass.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 527LD-33G Nylon 66, High Impact, 33% Glass Reinforced A high impact reinforced Nylon 66 with good low temperature properties.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66 A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 528L-13G Nylon 66, 13% Glass Reinforced General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur.. |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 528L2 Nylon 66 A general purpose highly lubricated Nylon 66 resin.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced Long glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provid.. |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 528L-5G Nylon 66, 5% Glass Reinforced General purpose glass fiber reinforced nylon, designed for parts requiring improved dimensional stability and higher strength than conventional resins.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufac.. |
|||
Melting Point | 252 °C | 486 °F | ASTM D789 |
Chem Polymer Chemlon 109 Nylon 66, High Impact A highly impact-modified, lubricated nylon 66 exhibiting excellent toughness, especially at lower temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 252 °C | 486 °F | ASTM D789 |
Chem Polymer Chemlon 182 Nylon 66, Flame Retarded A non-halogenated, unfilled nylon 66 used in electrical applications where improved flame retardancy is required. The material has excellent moldability, good snap-fit properties and is available i.. |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 520-13G Nylon 66, 13% Glass Reinforced 13% Glass reinforced Nylon 66.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 520-20GU Nylon 66, 20% Glass Reinforced 20% Glass reinforced Nylon 66, utility grade.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 520-25GU Nylon 66, 25% Glass Reinforced Nylon 66, 25% glass reinforced resin, utility grade.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 520-50G Nylon 66, 50% Glass Reinforced 50% Glass reinforced Nylon 66.Data provided by the manufacturer |
|||
Melting Point | 252 °C | 486 °F | ASTM D3418 |
Ashley Polymers Ashlene® 528SMS-30GB Nylon 66, 30% Glass Reinforced A 30% glass reinforced, heat stabilized, black Nylon 66 with Molybdenum disulfide.Data provided by the manufacturer |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 645 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 732 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co. |