Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.9 MPa | 6800 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP-8463-7001 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 46.9 - 159 MPa | 6800 - 23000 psi | Average value: 116 MPa Grade Count:41 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
I. Stern 108B Utility Black ABS Features:Good processing characteristicsInjection Molding and ExtrusionApplicationsProfilesPicture Frames, Tubes, RodsSpools, ReelsInformation provided by I. Stern & Co. Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Lucent Polymers PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES HiFill® TPX-PBT-01022 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D 638 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D 638 |
Styrolution PS 1621 GPPS Easy flow material with excellent moldabilityExcellent clarity and set-up timeInformation provided by Styrolution |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
PlastxWorld CEVIAN® E81 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM 638 |
PlastxWorld CEVIAN®-V 420 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 11 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D-638 |
Axiall 9211 Rigid PVC, Molding Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D-638 |
Axiall CL-7053 Rigid PVC, Molding Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM 638 |
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |