Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO179/3C DIN.53453
Omnia Plastica Akulon® PA 66 - Akulon 66 - Dry
Polyamide obtained by the polymerisation of Hexamethylenediamine and Adipic acid. It is one of the oldest engineering plastics, having been created in the USA in 1930. Due to its origin it is widely..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179-1
Polycasa XT 610 PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 N-V2 Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, low viscosity, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL A63 TF20 Nylon 6.6 for injection molding, 20% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179-1/1eA
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data)
This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein..
Charpy Impact, Notched 0.500 - 0.500 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.500 J/cm² Grade Count:1
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Charpy Impact, Notched 0.500 - 1.80 J/cm²

@Temperature -30.0 - 30.0 °C
2.38 - 8.57 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.993 J/cm² Grade Count:7
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 19-8195/FR Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® A1S25 H PA66 Heat Stabilized
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Kuraray Genestarâ„¢ N1002A-M41 Nylon
Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
LATI Latigray 82-04 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179/2C
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® M450-44/M450S Acetal Co-polymer (POM), Standard, Super high flow, High cycle
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179
Vyncolit X6952 Novolac Phenolic
Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn..
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Total PPC 7650 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 7650 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a medium fluidity offering a combination of ease of processing and excellent impact propert..
Charpy Impact, Notched 0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15
Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b..
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
BASF Novolen® 1102 H Polypropylene
Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Conditioned; ISO 179/IeA
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
Charpy Impact, Notched 0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
ISO 179/1eA
Celanese Celanex® 3200HR PBT, 15% Glass Reinforced
Celanex 3200HR is a 15% glass filled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degradation during processi..
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
LATI Latimass 47/7-04 D008 PP Copolymer
Specific density compound based on Polypropylene copolymer (PPc). Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In..
Charpy Impact, Notched 0.500 J/cm²

@Temperature -40.0 °C
2.38 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET  (Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont
Charpy Impact, Notched 0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TS FR PA666 FR
Information provided by EMS Grivory
Copyright © lookpolymers.com All Rights Reserved