Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.96 - 103 MPa | 720 - 15000 psi | Average value: 81.3 MPa Grade Count:31 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant PA131 Nylon 66, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6253 Nylon 6, High Impact Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA111 Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PBT1100S Polybutylene Terephthalate, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0006GY-371 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPSP0004 Polypropylene, Random Copolymer Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPT10 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol TPU2087AFR Polyurethane Elastomer, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant PA223 Nylon 6, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPSSP0006 Polyphenylene Sulfide, Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 103 MPa | 720 - 15000 psi | Average value: 83.0 MPa Grade Count:51 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |