Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.9 MPa | 6800 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP-8463-7001 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 46.9 - 159 MPa | 6800 - 23000 psi | Average value: 116 MPa Grade Count:41 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Global GPP-220-C 20% Glass Reinforced, Chemically Coupled Impact Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES HiFill® TPX-PBT-01022 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D 638 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D 638 |
Styrolution PS 1611 GPPS Injection moldingGood balance of flow, strength and set-up propertiesUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
PlastxWorld CEVIAN® E81 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM 638 |
PlastxWorld CEVIAN® LMW48 Laser Markable Grade ABS White MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 11 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D-638 |
Axiall 9211 Rigid PVC, Molding Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG.. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM 638 |
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM Data |
Styron Magnum™ 9100 MFD ABS Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010. |