Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.12 g/cc | 0.0405 lb/in³ | |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet TangoBlack FullCure970 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**) Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into.. |
|||
Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | |
Fibre Glast 2000 / 2120 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | DIN 53479 |
Kraiburg TPE THERMOLAST® K TS7ADZ Black TPE Black compound for applications with reduced requirementsTypical Applications: GripsErasersGrips on stationeriesTransport protectionAnti-slip elementsSkirting boardMaterial Advantages: Excellent pri.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183/A |
Grupo Repol Dinalon® B1S25 MI PA6 Medium Impact Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East) LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Density | 1.12 - 1.14 g/cc | 0.0405 - 0.0412 lb/in³ | ASTM D792 |
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, 50% RH Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® BRZ 234/1 W PA6 Grilon BRZ 234/1 W is a modified polyamide 6, suitable for tube extrusion. Grilon BRZ 234/1 W is heat stabilized, shows a high flexibility and high impact strength. It is especially developed for th.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
Arkema Group Orgalloy® RS 6010 Nylon 6 Alloy, 10% Glass Fiber Reinforced (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene HP0335G30CHIV Homopolymer Glass Reinforced High Impact Coupled Approved to GMP.PP.017 Black A12563 |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
BASF Procom® GC30S 401 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
BASF Procom® GC30S 403 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | |
Arkema Group Appryl® CZN 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for interior trim applications, that required an excellent impact test associated with a high modul.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 850 Nylon 6 This is an extrusion grade Nylon 6 resin suitable for both coextrusion and blown film applications. It has excellent melt stability and very high melt strength. It also has excellent grease resist.. |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |
|||
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10 LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive. |