Polymer Property : Linear Mold Shrinkage, Transverse = 0.0130 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0114 - 0.0130 cm/cm
0.0114 - 0.0130 in/in
Average value: 0.0122 cm/cm Grade Count:4
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0130 cm/cm
0.00500 - 0.0130 in/in
Average value: 0.00821 cm/cm Grade Count:37
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0130 cm/cm
0.00700 - 0.0130 in/in
Average value: 0.00929 cm/cm Grade Count:14
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Linear Mold Shrinkage, Transverse 0.000 - 0.0130 cm/cm
0.000 - 0.0130 in/in
Average value: 0.00702 cm/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0130 cm/cm
0.00200 - 0.0130 in/in
Average value: 0.00812 cm/cm Grade Count:47
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..