Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Mold Temperature | 50.0 °C | 122 °F | |
Northstar Polymers MPP-A80H Room-Temperature Curable Polyurethane MPP-A80H has been specifically formulated to service applications where high elongation and good physical strength are required as well as where temperature during the process must be low for a very.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Mold Temperature | 50.0 - 104 °C | 122 - 220 °F | Average value: 79.5 °C Grade Count:29 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | |
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Mold Temperature | 50.0 - 120 °C | 122 - 248 °F | |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Staramide 6 80E7 PA6, Injection Molded Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Starflam PX06010 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06010 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
BASF Elastollan R 3001 15% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Asia International Enterprise (Hong Kong) 60G5F Nylon 66, 25% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Injection Molding |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Injection Molding |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Asia International Enterprise (Hong Kong) 60T6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Injection Molding |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | DAM |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app.. |