Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ISO 8302 |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 23.0 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM D1269E |
Premix Premi-Glas® 2200-22 Fiberglass Reinforced SMC
(discontinued **) Description: Premi-Glas® 2200-22 is a fiberglass reinforced thermoset Sheet Molding Compound similar to the Premi-Glas® 2200-22 CR-SX product. Unlike the -CR-SX version, this product carries no UL.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM D1269E |
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50/CF/7/GS/10/TF/5/EM/BK Polycarbonate, with carbon fiber, glass flakes and PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM E1530 |
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moistu.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | Silicone Property; Arlon SQA-TMS-022 |
Arlon R36812T010 0.010" Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorin.. |