Processing Properties Metric English Comments
Mold Temperature 80.0 - 110 °C
176 - 230 °F
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Preferred
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Preferred
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Preferred
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
Mold Temperature 10.0 - 110 °C
50.0 - 230 °F
Average value: 39.5 °C Grade Count:416
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Mold Temperature 82.2 - 110 °C
180 - 230 °F
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 90.0 - 110 °C
194 - 230 °F
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Preferred
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
Mold Temperature 70.0 - 110 °C
158 - 230 °F
DAM
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface
Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Mold Temperature 70.0 - 110 °C
158 - 230 °F
LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUPOY SC1004A PC
Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Mold Temperature 60.0 - 110 °C
140 - 230 °F
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled
Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET
Information provided by A. Schulman.
Mold Temperature 60.0 - 110 °C
140 - 230 °F
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural
Information provided by Eurotec®
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NA40 GR30 NL HW PA6.6, 30% glass fiber reinforced, hydrolysis stabilized, natural
Information provided by Eurotec®
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NA40 KG30 NL 0B PA6.6, 30% glass fiber/glass bead reinforced, natural
Information provided by Eurotec®
Mold Temperature 60.0 - 110 °C
140 - 230 °F
Eurotec® Tecodur® PB70 GR30 NL100 HT01 PBT, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec®
Mold Temperature 80.0 - 110 °C
176 - 230 °F
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Kraiburg TPE THERMOLAST® K TC6HAZ Black TPE  (Unverified Data**)
Adhesion to POM (Hostaform®, Duracon, Celcon)Patented system for TPE-S and POMEasy processabilityBroad service temperature rangeTypical Applications: Hard/soft applications with POM:SealingOver mol..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Kraiburg TPE THERMOLAST® K TC7HBZ Black TPE  (Unverified Data**)
Adhesion to POM (Hostaform®, Duracon, Celcon)Patented system for TPE-S and POMEasy processabilityBroad service temperature rangeTypical Applications: Hard/soft applications with POM:SealingOver mol..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
LATI Latilub 95-15T PSU, PTFE Filled
Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..