Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.50 - 8.70 J/cm² @Temperature -30.0 - -30.0 °C |
16.7 - 41.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.29 J/cm² Grade Count:9 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact Unnotched | 0.400 - 8.70 J/cm² @Temperature -40.0 - -20.0 °C |
1.90 - 41.4 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.42 J/cm² Grade Count:56 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |