Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 52.0 - 95.0 kJ/m²

@Temperature -30.0 - -30.0 °C
24.7 - 45.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 75.0 kJ/m² Grade Count:5
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Izod Impact, Unnotched (ISO) 45.0 - 95.0 kJ/m²
21.4 - 45.2 ft-lb/in²
Average value: 72.0 kJ/m² Grade Count:18
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched (ISO) 10.0 - 95.0 kJ/m²
4.76 - 45.2 ft-lb/in²
Average value: 47.8 kJ/m² Grade Count:19
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Unnotched (ISO) 50.0 - 95.0 kJ/m²

@Temperature -30.0 - -30.0 °C
23.8 - 45.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 75.8 kJ/m² Grade Count:6
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Izod Impact, Unnotched (ISO) 65.0 - 95.0 kJ/m²
30.9 - 45.2 ft-lb/in²
Average value: 82.2 kJ/m² Grade Count:7
Overview of materials for Nylon 610, Glass Reinforced