Polymer Property : Mold Temperature = 110 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 10.0 - 110 °C
50.0 - 230 °F
Injection Molding
DuPont Performance Polymers Crastin® CE15315 BK010 PBT  (Unverified Data**)
Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
Mold Temperature 82.2 - 110 °C
180 - 230 °F
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Preferred
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Preferred
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte..
Mold Temperature 79.0 - 110 °C
174 - 230 °F
Albis Plastics Polyamide 6/66 PA 152 GF30/02 BK8-1114 Black 30% Glass Fiber  (discontinued **)
Semi-crystalline Nylon 6/66 (PA6/66)Characteristics: Industrial GradeApplications: Office Furniture, Gear, Housings and ConnectorsProcessing: Injection Molding (Melt Temperature: 465 -555°F, Mold ..
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Lehmann & Voss LUVOCOM® 6-8211 Polyamide 12, with glass fiber, thermally conductive modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Low waterabsorbtion, for d..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Start Point: 90°C
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact
Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUMID SG4389B PA66+GF/MF38%
Feature: Injection Molding, PA66+GF/MF38%Application: Automotive (Fan & Shroud)CAS No. 32131-17-2, 25038-54-4, 65997-17-3 and 14807-96-6Information provided by LG Chemical
Mold Temperature 70.0 - 110 °C
158 - 230 °F
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUPOY SC1004A PC
Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
LATI Latilub 87/28-17ST K/15 PC, 15% Carbon Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polycarbonate (PC). Silicone / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Mold Temperature 65.6 - 110 °C
150 - 230 °F
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40..
Mold Temperature 77.0 - 110 °C
171 - 230 °F
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
Mold Temperature 90.0 - 110 °C
194 - 230 °F
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET
Information provided by A. Schulman.
Mold Temperature 90.0 - 110 °C
194 - 230 °F
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Mold Temperature 54.4 - 110 °C
130 - 230 °F
Average value: 76.3 °C Grade Count:16
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Mold Temperature 60.0 - 110 °C
140 - 230 °F
Suzhou Hipro Polymers Hiprolon® 90 MC HLS G30 Nylon 612, 30% glass fiber filled
Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resi..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Kraiburg TPE THERMOLAST® K TC7HAA Natural TPE  (Unverified Data**)
Adhesion to POM (Hostaform®, Duracon, Celcon)Patented system for TPE-S and POMEasy processabilityBroad service temperature rangeTypical Applications: Hard/soft applications with POM:SealingOver mol..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Kraiburg TPE THERMOLAST® K TC6HAZ Black TPE  (Unverified Data**)
Adhesion to POM (Hostaform®, Duracon, Celcon)Patented system for TPE-S and POMEasy processabilityBroad service temperature rangeTypical Applications: Hard/soft applications with POM:SealingOver mol..