Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.962 - 1.54 g/cc
0.0348 - 0.0555 lb/in³
Average value: 1.29 g/cc Grade Count:107
1.02 - 1.07 g/cc

@Temperature 260 - 260 °C
0.0368 - 0.0387 lb/in³

@Temperature 500 - 500 °F
Average value: 1.05 g/cc Grade Count:2
Filler Content 5.00 - 40.0 %
5.00 - 40.0 %
Average value: 19.1 % Grade Count:26
Water Absorption 0.0570 - 0.700 %
0.0570 - 0.700 %
Average value: 0.233 % Grade Count:31
Moisture Absorption at Equilibrium 0.0400 - 0.320 %
0.0400 - 0.320 %
Average value: 0.174 % Grade Count:27
Water Absorption at Saturation 0.600 - 0.700 %
0.600 - 0.700 %
Average value: 0.611 % Grade Count:9
Maximum Moisture Content 0.0200 - 0.0400
0.0200 - 0.0400
Average value: 0.0240 Grade Count:5
Linear Mold Shrinkage 0.000500 - 0.00700 cm/cm
0.000500 - 0.00700 in/in
Average value: 0.00298 cm/cm Grade Count:87
Linear Mold Shrinkage, Transverse 0.00150 - 0.00800 cm/cm
0.00150 - 0.00800 in/in
Average value: 0.00441 cm/cm Grade Count:23
Melt Flow 1.00 - 37.0 g/10 min
1.00 - 37.0 g/10 min
Average value: 12.9 g/10 min Grade Count:34
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82.0 - 121
82.0 - 121
Average value: 116 Grade Count:24
Hardness, H358/30 116 MPa
16800 psi
Average value: 116 MPa Grade Count:4
Tensile Strength, Ultimate 27.0 - 156 MPa
3920 - 22600 psi
Average value: 87.9 MPa Grade Count:87
5.00 - 50.0 MPa

@Temperature 60.0 - 120 °C
725 - 7250 psi

@Temperature 140 - 248 °F
Average value: 26.0 MPa Grade Count:1
Tensile Strength, Yield 48.8 - 156 MPa
7080 - 22600 psi
Average value: 92.5 MPa Grade Count:41
Elongation at Break 0.600 - 109 %
0.600 - 109 %
Average value: 4.22 % Grade Count:92
3.00 - 70.0 %

@Temperature 60.0 - 120 °C
3.00 - 70.0 %

@Temperature 140 - 248 °F
Average value: 26.3 % Grade Count:1
Elongation at Yield 0.900 - 4.00 %
0.900 - 4.00 %
Average value: 2.37 % Grade Count:26
2.00 - 2.00 %

@Temperature 60.0 - 120 °C
2.00 - 2.00 %

@Temperature 140 - 248 °F
Average value: 2.00 % Grade Count:1
Modulus of Elasticity 3.30 - 20.3 GPa
479 - 2940 ksi
Average value: 6.89 GPa Grade Count:65
1.30 - 3.60 GPa

@Temperature 60.0 - 120 °C
189 - 522 ksi

@Temperature 140 - 248 °F
Average value: 2.73 GPa Grade Count:1
Flexural Yield Strength 57.0 - 224 MPa
8270 - 32500 psi
Average value: 132 MPa Grade Count:90
Flexural Modulus 3.00 - 12.9 GPa
435 - 1870 ksi
Average value: 5.99 GPa Grade Count:97
Izod Impact, Notched 0.278 - 3.04 J/cm
0.520 - 5.70 ft-lb/in
Average value: 1.14 J/cm Grade Count:79
0.440 - 3.20 J/cm

@Temperature -50.0 - 0.000 °C
0.824 - 5.99 ft-lb/in

@Temperature -58.0 - 32.0 °F
Average value: 1.44 J/cm Grade Count:19
Izod Impact, Unnotched 0.747 - 8.01 J/cm
1.40 - 15.0 ft-lb/in
Average value: 5.35 J/cm Grade Count:40
3.30 - 6.04 J/cm

@Temperature -40.0 - -30.0 °C
6.18 - 11.3 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 4.39 J/cm Grade Count:7
Izod Impact, Notched (ISO) 4.00 - 28.0 kJ/m²
1.90 - 13.3 ft-lb/in²
Average value: 15.2 kJ/m² Grade Count:31
5.00 - 34.0 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 16.2 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 17.3 kJ/m² Grade Count:16
Izod Impact, Unnotched (ISO) 15.0 - 70.0 kJ/m²
7.14 - 33.3 ft-lb/in²
Average value: 35.2 kJ/m² Grade Count:26
21.0 - 52.0 kJ/m²

@Temperature -40.0 - -30.0 °C
9.99 - 24.7 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 32.0 kJ/m² Grade Count:7
Charpy Impact Unnotched 1.50 - 9.00 J/cm²
7.14 - 42.8 ft-lb/in²
Average value: 4.07 J/cm² Grade Count:9
3.00 - 4.40 J/cm²

@Temperature -40.0 - -20.0 °C
14.3 - 20.9 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.63 J/cm² Grade Count:3
Charpy Impact, Notched 0.300 - 3.20 J/cm²
1.43 - 15.2 ft-lb/in²
Average value: 0.979 J/cm² Grade Count:21
0.300 - 1.20 J/cm²

@Temperature -40.0 - 0.000 °C
1.43 - 5.71 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 0.633 J/cm² Grade Count:10
Dart Drop, Total Energy 11.0 - 35.0 J
8.11 - 25.8 ft-lb
Average value: 18.1 J Grade Count:19
8.00 - 19.0 J

@Temperature -30.0 - -30.0 °C
5.90 - 14.0 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 13.5 J Grade Count:2
Falling Dart Impact 52.877 - 52.877 J

@Temperature -28.9 - -28.9 °C
39.000 - 39.000 ft-lb

@Temperature -20.0 - -20.0 °F
Average value: 52.9 J Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 18.0 - 77.4 µm/m-°C
10.0 - 43.0 µin/in-°F
Average value: 40.8 µm/m-°C Grade Count:46
CTE, linear, Transverse to Flow 32.0 - 90.0 µm/m-°C
17.8 - 50.0 µin/in-°F
Average value: 58.3 µm/m-°C Grade Count:31
Specific Heat Capacity 1.56 - 2.15 J/g-°C
0.373 - 0.514 BTU/lb-°F
Average value: 1.82 J/g-°C Grade Count:5
Thermal Conductivity 0.142 - 0.260 W/m-K
0.985 - 1.80 BTU-in/hr-ft²-°F
Average value: 0.194 W/m-K Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 146 °C
198 - 295 °F
Average value: 130 °C Grade Count:47
Deflection Temperature at 1.8 MPa (264 psi) 53.0 - 160 °C
127 - 320 °F
Average value: 120 °C Grade Count:93
Vicat Softening Point 93.0 - 144 °C
199 - 291 °F
Average value: 126 °C Grade Count:36
UL RTI, Electrical 60.0 °C
140 °F
Average value: 60.0 °C Grade Count:10
UL RTI, Mechanical with Impact 60.0 °C
140 °F
Average value: 60.0 °C Grade Count:10
Electrical Properties Metric English Comments
Electrical Resistivity 10000 - 3.50e+16 ohm-cm
10000 - 3.50e+16 ohm-cm
Average value: 5.54e+15 ohm-cm Grade Count:26
Surface Resistance 1000 - 3.50e+16 ohm
1000 - 3.50e+16 ohm
Average value: 2.92e+15 ohm Grade Count:18
Dielectric Constant 2.80 - 3.40
2.80 - 3.40
Average value: 3.12 Grade Count:9
Dielectric Strength 27.0 - 40.0 kV/mm
686 - 1020 kV/in
Average value: 31.3 kV/mm Grade Count:11
Dissipation Factor 0.00200 - 0.0110
0.00200 - 0.0110
Average value: 0.00594 Grade Count:9
Comparative Tracking Index 150 - 350 V
150 - 350 V
Average value: 215 V Grade Count:10
Copyright © lookpolymers.com All Rights Reserved