Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 295 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 146 °C
198 - 295 °F
Average value: 130 °C Grade Count:47
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Deflection Temperature at 0.46 MPa (66 psi) 132 - 146 °C
270 - 295 °F
Average value: 139 °C Grade Count:13
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Deflection Temperature at 0.46 MPa (66 psi) 91.1 - 146 °C
196 - 295 °F
Average value: 137 °C Grade Count:16
Overview of materials for Polycarbonate, Stainless Steel Fiber