Polymer Property : Specific Heat Capacity = 0.373 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.56 - 2.15 J/g-°C
0.373 - 0.514 BTU/lb-°F
Average value: 1.82 J/g-°C Grade Count:5
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Specific Heat Capacity 1.56 J/g-°C
0.373 BTU/lb-°F
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite
Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif..
Specific Heat Capacity 1.56 J/g-°C

@Temperature 20.0 °C
0.373 BTU/lb-°F

@Temperature 68.0 °F
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) ..
Specific Heat Capacity 1.56 J/g-°C
0.373 BTU/lb-°F
Melt
Covestro Bayblend® T88 GF-20* Polycarbonate + SAN Glass Filled Impact Grade
Developmental productInjection molding grade20 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 7500 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content
Specific Heat Capacity 1.56 J/g-°C
0.373 BTU/lb-°F
Melt
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
Injection molding grade20 % glass fiber filledtensile modulus = 5900 MPaVicat/B 120 temperature = 134 °CPreprocessingMax. Water content
Specific Heat Capacity 1.56 J/g-°C

@Temperature 20.0 °C
0.373 BTU/lb-°F

@Temperature 68.0 °F
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..
Specific Heat Capacity 1.56 J/g-°C

@Temperature 20.0 °C
0.373 BTU/lb-°F

@Temperature 68.0 °F
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are..