Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® G320 ABS (Europe-Africa-Middle East) CYCOLAC G320 is a super high impact resistant ABS grade. It combines impact resistance with high stiffness, good temperature resistance and processability. It has a good fit in automotive interiors .. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | DIN 53460 |
Ineos Nova S-3500MG Compact Polystyrene Microgranulates
(discontinued **) Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and .. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ASTM D1525 |
Huntsman PE5030 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | 50°C/h 50N |
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B120; ISO 306 |
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | resin; ASTM D1525 |
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | VST/B/50; ISO 306 |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 93.0 °C | 199 °F | 50B; ISO 306 |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ASTM D1525 |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | 120°C/hr, 9.8N; ASTM D1525 |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
Vicat Softening Point | 93.0 °C | 199 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | |
Dow LDPE 993I Low Density Polyethylene DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability .. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ASTM D1525 |
Huntsman PE2060 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High flow characteristics, good processability.Applications: Injection molding: general purpose molding, large moldings including housewares and toys.FDA Note.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ASTM D648 |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP 6630 Antistatic Polystyrene Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti.. |