Electrical Properties Metric English Comments
Electrical Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
dry; IEC 60093
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive
Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•..
Electrical Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
IEC 60093
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive
Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
Nabaltec APYRAL® 120E Al(OH)3
APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio..
Electrical Resistivity 10000 - 1.00e+16 ohm-cm
10000 - 1.00e+16 ohm-cm
Average value: 4.21e+15 ohm-cm Grade Count:6
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and ..
Electrical Resistivity 10000 - 1.00e+16 ohm-cm
10000 - 1.00e+16 ohm-cm
Average value: 1.10e+15 ohm-cm Grade Count:33
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Electrical Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D257
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 10000 - 3.50e+16 ohm-cm
10000 - 3.50e+16 ohm-cm
Average value: 5.54e+15 ohm-cm Grade Count:26
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Electrical Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
ASTM D257
PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® 25CAR+5CER PTFE; Petroleum Coke and Ceramic Filled  (discontinued **)
Data provided by the manufacturer.25 wt.% Petroleum Coke + 5 wt.% Ceramic. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectr..
Electrical Resistivity 10000 - 1.00e+15 ohm-cm
10000 - 1.00e+15 ohm-cm
Average value: 8.57e+14 ohm-cm Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Electrical Resistivity 10000 - 1.00e+18 ohm-cm
10000 - 1.00e+18 ohm-cm
Average value: 1.87e+17 ohm-cm Grade Count:44
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Electrical Resistivity 10000 - 8.10e+16 ohm-cm
10000 - 8.10e+16 ohm-cm
Average value: 6.23e+15 ohm-cm Grade Count:13
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
IEC 60093
3M Dyneon™ TF 4220 PTFE 2% Cond. Pigm. Filled  (discontinued **)
Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon.
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
IEC 60093
3M Dyneon™ TF 4406 PTFE, 60% Bronze Filled  (discontinued **)
Type II PTFE. Applications include sliding surfaces, bearings.Data provided by Dyneon.
Electrical Resistivity 10000 - 1.00e+17 ohm-cm
10000 - 1.00e+17 ohm-cm
Average value: 1.28e+16 ohm-cm Grade Count:45
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Electrical Resistivity 10000 - 1.00e+15 ohm-cm
10000 - 1.00e+15 ohm-cm
Average value: 2.14e+14 ohm-cm Grade Count:10
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
Average
Shakespeare Sanstat® CN125 .28mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
Electrical Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
Shakespeare Sanstat® CN125 .41mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
Specific Resistance
UBE Tyranno Grade C Ceramic Semi-Conductive Fiber
Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned)
Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No ..
Electrical Resistivity 10000 - 1.00e+20 ohm-cm
10000 - 1.00e+20 ohm-cm
Average value: 5.21e+18 ohm-cm Grade Count:20
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® 25CAR PTFE; Petroleum Coke and Graphite  (discontinued **)
Data provided by the manufacturer.25 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
Arkema Group Kynar® 6000 HDC N 119 PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie..
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
IEC 60093
3M Dyneon™ TFM™ 4220 Modified PTFE, 2% Cond. Pigm. Filled  (discontinued **)
Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon.
Electrical Resistivity 10000 - 8.00e+15 ohm-cm
10000 - 8.00e+15 ohm-cm
Average value: 4.20e+14 ohm-cm Grade Count:56
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Electrical Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
ASTM D257
PolyOne Edgetek® ES-06CF-09GF/000 RED Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications &
Data provided by PolyOne.
Electrical Resistivity 10000 - 2.00e+14 ohm-cm
10000 - 2.00e+14 ohm-cm
Average value: 5.91e+13 ohm-cm Grade Count:30
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Copyright © lookpolymers.com All Rights Reserved