Thermal Properties Metric English Comments
Thermal Conductivity 0.142 - 0.260 W/m-K
0.985 - 1.80 BTU-in/hr-ft²-°F
Average value: 0.194 W/m-K Grade Count:10
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Thermal Conductivity 0.142 W/m-K
0.985 BTU-in/hr-ft²-°F
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced
PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used..
Thermal Conductivity 0.142 W/m-K
0.985 BTU-in/hr-ft²-°F
Dow Corning XIAMETER® PMCPPMX-200 20Cs Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 20CS. 100% active, 20 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Thermal Conductivity 0.142 W/m-K
0.985 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T45 PG Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °Cfor electroplating applicationsPreprocessingMax. Water content
Thermal Conductivity 0.142 W/m-K
0.985 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T45 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content
Thermal Conductivity 0.142 W/m-K
0.985 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T50 XF Polycarbonate + ABS
Injection molding gradeVicat/B 120 = 115 °Cexcellent flowgood low temperature impact strengthPreprocessingMax. Water content