Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.00 - 4.40 J/cm²

@Temperature -40.0 - -20.0 °C
14.3 - 20.9 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.63 J/cm² Grade Count:3
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Charpy Impact Unnotched 1.00 - 4.40 J/cm²
4.76 - 20.9 ft-lb/in²
Average value: 2.14 J/cm² Grade Count:20
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..