Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² - NB | 7.14 ft-lb/in² - NB | Average value: 129 kJ/m² Grade Count:51 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 70.0 kJ/m² | 7.14 - 33.3 ft-lb/in² | Average value: 35.2 kJ/m² Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 20.0 kJ/m² | 7.14 - 9.52 ft-lb/in² | Average value: 17.7 kJ/m² Grade Count:3 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 56.6 kJ/m² | 7.14 - 26.9 ft-lb/in² | Average value: 34.8 kJ/m² Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 80.0 kJ/m² | 7.14 - 38.1 ft-lb/in² | Average value: 34.0 kJ/m² Grade Count:18 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL6013T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RL0039XP PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RL0039XP is a compound based on PA66 resin containing PTFE, Flame Retardant. Added features include ; Flame Retardant, internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX01075 is a compound based on Nylon 66 resin containing PTFE, Mineral. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon OX92182 PPS (Europe-Africa-Middle East) LNP* STAT-KON* OX92182 is a compound based on PPS-Branched resin containing Glass Fiber, Carbon Fiber, Mineral. Added features include : Electrically Conductive.This data was supplied by SABIC-IP fo.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON ZEF061XC PPO (Europe-Africa-Middle East) LNP* STATKON* ZEF061XC is a compound based on Polyphenyleneoxide resin containing Glass Fiber, Milled Carbon Fiber and Flame Retardant. Added Features include: Electrically Conductive |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AF004 is a compound based on Acrylonitrile Butadiene Styren resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MFB44S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFB44S is a compound based on Polypropylene resin containing Glass Fiber, Glass Beads. Added features include; Heat Stabilized, Cu-Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1C |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1C |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1C |
Chi Mei Kibisan® PN-117 SAN Injection Molding |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0069 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding Resin (also known as Starflam PA6 30E6 Z88)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NTFA Homopolymer 20% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 98.0 kJ/m² | 7.14 - 46.6 ft-lb/in² | Average value: 56.2 kJ/m² Grade Count:10 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KEL32 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL32 is a compound based on Acetal Copolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² - NB | 7.14 ft-lb/in² - NB | Average value: 59.7 kJ/m² Grade Count:9 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |