Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.142 - 0.260 W/m-K | 0.985 - 1.80 BTU-in/hr-ft²-°F | Average value: 0.194 W/m-K Grade Count:10 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Thermal Conductivity | 0.225 - 0.259 W/m-K | 1.56 - 1.80 BTU-in/hr-ft²-°F | Average value: 0.250 W/m-K Grade Count:8 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Thermal Conductivity | 0.245 - 0.259 W/m-K | 1.70 - 1.80 BTU-in/hr-ft²-°F | Average value: 0.252 W/m-K Grade Count:4 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |