Polymer Property : Tensile Strength, Ultimate = 7250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 32.0 - 50.0 MPa

@Temperature 60.0 - 120 °C
4640 - 7250 psi

@Temperature 140 - 248 °F
Average value: 41.7 MPa Grade Count:1
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Tensile Strength, Ultimate 5.00 - 50.0 MPa

@Temperature 60.0 - 120 °C
725 - 7250 psi

@Temperature 140 - 248 °F
Average value: 26.0 MPa Grade Count:1
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 30.0 - 50.0 MPa
4350 - 7250 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer  (discontinued **)
Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P..
Tensile Strength, Ultimate 6.89 - 50.0 MPa
1000 - 7250 psi
Average value: 20.3 MPa Grade Count:68
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Tensile Strength, Ultimate 35.0 - 50.0 MPa
5080 - 7250 psi
Average value: 43.8 MPa Grade Count:16
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Ultimate 31.0 - 50.0 MPa
4500 - 7250 psi
Average value: 40.8 MPa Grade Count:9
Overview of materials for Nylon 12, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 40.0 - 50.0 MPa
5800 - 7250 psi
ASTM D638
Zeus EFEP Tubing
Tensile Strength, Ultimate 37.0 - 50.0 MPa
5370 - 7250 psi
ASTM D638
Zeus ETFE Tubing
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess..
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 20.0 - 50.0 MPa
2900 - 7250 psi
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material
Tensile Strength, Ultimate 35.0 - 50.0 MPa
5080 - 7250 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer  (discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Tensile Strength, Ultimate 35.0 - 50.0 MPa
5080 - 7250 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer  (discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
Tensile Strength, Ultimate 35.0 - 50.0 MPa
5080 - 7250 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer  (discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Tensile Strength, Ultimate 35.0 - 50.0 MPa
5080 - 7250 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer  (discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
Tensile Strength, Ultimate 30.0 - 50.0 MPa
4350 - 7250 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer  (discontinued **)
Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Tensile Strength, Ultimate 13.0 - 50.0 MPa
1890 - 7250 psi
Average value: 27.6 MPa Grade Count:116
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Tensile Strength, Ultimate 33.0 - 50.0 MPa

@Temperature 60.0 - 120 °C
4790 - 7250 psi

@Temperature 140 - 248 °F
Average value: 41.0 MPa Grade Count:1
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..