Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 21.0 - 52.0 kJ/m² @Temperature -40.0 - -30.0 °C |
9.99 - 24.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 32.0 kJ/m² Grade Count:7 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Unnotched (ISO) | 45.0 - 52.0 kJ/m² | 21.4 - 24.7 ft-lb/in² | Average value: 48.3 kJ/m² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 - 52.0 kJ/m² | 19.5 - 24.7 ft-lb/in² | Average value: 46.3 kJ/m² Grade Count:4 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |