Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.142 - 0.260 W/m-K | 0.985 - 1.80 BTU-in/hr-ft²-°F | Average value: 0.194 W/m-K Grade Count:10 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |