Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature 20.0 °C
17.8 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
CTE, linear, Transverse to Flow 32.0 - 90.0 µm/m-°C
17.8 - 50.0 µin/in-°F
Average value: 58.3 µm/m-°C Grade Count:31
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
CTE, linear, Transverse to Flow 32.0 - 45.0 µm/m-°C
17.8 - 25.0 µin/in-°F
Average value: 38.0 µm/m-°C Grade Count:5
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature 20.0 °C
17.8 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer
LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
CTE, linear, Transverse to Flow 32.0 µm/m-°C
17.8 µin/in-°F
TMA
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic
Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is requiredInformation provided by Sumitomo Bak North America, Inc.
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature 20.0 °C
17.8 µin/in-°F

@Temperature 68.0 °F
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Thickness 1.60 mm
17.8 µin/in-°F

@Thickness 0.0630 in
ASTM D696
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Verton UX06451 PPA
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
CTE, linear, Transverse to Flow 32.0 - 32.0 µm/m-°C

@Temperature 55.0 - 160 °C
17.8 - 17.8 µin/in-°F

@Temperature 131 - 320 °F
Average value: 32.0 µm/m-°C Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
CTE, linear, Transverse to Flow 32.0 µm/m-°C
17.8 µin/in-°F
ASTM E831
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information ..
CTE, linear, Transverse to Flow 32.0 - 2780 µm/m-°C
17.8 - 1540 µin/in-°F
Average value: 118 µm/m-°C Grade Count:36
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
CTE, linear, Transverse to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Copyright © lookpolymers.com All Rights Reserved