Polymer Property : Density = 0.0387 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.03 - 1.07 g/cc
0.0372 - 0.0387 lb/in³
Average value: 1.04 g/cc Grade Count:64
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Density 1.02 - 1.07 g/cc

@Temperature 260 - 260 °C
0.0368 - 0.0387 lb/in³

@Temperature 500 - 500 °F
Average value: 1.05 g/cc Grade Count:2
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Density 1.07 - 1.07 g/cc

@Temperature 270 - 270 °C
0.0387 - 0.0387 lb/in³

@Temperature 518 - 518 °F
Average value: 1.07 g/cc Grade Count:1
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Density 1.00 - 1.07 g/cc
0.0361 - 0.0387 lb/in³
Average value: 1.03 g/cc Grade Count:7
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Density 1.01 - 1.07 g/cc
0.0365 - 0.0387 lb/in³
ASTM D 792
Karina E 4048/1-TRE Kariprene Black
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 1.04 - 1.07 g/cc
0.0376 - 0.0387 lb/in³
Trelleborg Emerson & Cuming Eccobond® 45C Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45C Eccobond® Two-Component General Purpose Epoxy AdhesiveClear, unfilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the ..
Density 1.03 - 1.07 g/cc
0.0372 - 0.0387 lb/in³
Internal
AKG Polymers Vision PP PPC BL1010 T20 Polypropylene Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Density 1.02 - 1.07 g/cc
0.0368 - 0.0387 lb/in³
Part B
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg..
Density 1.02 - 1.07 g/cc
0.0368 - 0.0387 lb/in³
Part B
3M Scotch-Weld™ DP600NS Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600NS is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a tri..
Density 1.02 - 1.07 g/cc
0.0368 - 0.0387 lb/in³
Part B
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Density 1.02 - 1.07 g/cc
0.0368 - 0.0387 lb/in³
Part B
3M Scotch-Weld™ DP601NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Density 1.07 - 1.07 g/cc

@Temperature 270 - 270 °C
0.0387 - 0.0387 lb/in³

@Temperature 518 - 518 °F
Average value: 1.07 g/cc Grade Count:1
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Copyright © lookpolymers.com All Rights Reserved