| BASF Gusspolyamid® Nylon 6 (At 50% RH) |
Nylon 6, Unreinforced |
Gusspolyamid®
|
| BASF Gusspolyamid® Nylon 6 (Dry As Molded) |
Nylon 6, Unreinforced |
Gusspolyamid®
|
| BASF Nypel® 6015G HS BK 15% Glass Filled PA6 (Dry) |
Nylon 6, 20% Glass Fiber Filled |
Nypel®
|
| BASF Nypel® 6030G HS BK 30% Glass Filled PA6 (Dry) |
Renewable/Recycled Polymer |
Nypel®
|
| BASF Nypel® RC6024 BK 30% Mineral/Glass Filled PA6 (Dry) |
Renewable/Recycled Polymer |
Nypel®
|
| BASF Nypel® RC6030F BK 30% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Nypel®
|
| BASF Ultramid® 8200 HS PA 6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8200 HS PA 6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8202 HS BK-102 PA6 (Conditioned) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202 HS BK-102 PA6 (Dry) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202 HS PA6 (Conditioned) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202 HS PA6 (Dry) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8202 L Intermediate PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8202 PA6 (Conditioned) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202 PA6 (Dry) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202C HS BK-102 PA6 (Conditioned) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202C HS BK-102 PA6 (Dry) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202C HS PA6 (Conditioned) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202C HS PA6 (Dry) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202C PA6 (Conditioned) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202C PA6 (Dry) |
Nylon 6, Unreinforced, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8202CQ PA6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8202CQ PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned) |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry) |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Ultramid®
|
| BASF Ultramid® 8232G HS FR BK-102 25% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Conditioned) |
Nylon 6, 50% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry) |
Nylon 6, 50% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned) |
Nylon 6, 40% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) |
Nylon 6, 40% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Conditioned) |
Nylon 6, 40% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) |
Nylon 6, 40% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8253 BK-102 PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8253 HS BK-102 PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8253 HS PA6 (Conditioned) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8253 HS PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8253 PA6 (Conditioned) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8253 PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8254 HS BK-102 PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8255 HS PA6 (Conditioned) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8255 HS PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8260 40% Mineral Filled PA6 (Conditioned) |
Nylon 6, 40% Mineral Filled |
Ultramid®
|
| BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry) |
Nylon 6, 40% Mineral Filled |
Ultramid®
|
| BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned) |
Nylon 6, 40% Mineral Filled |
Ultramid®
|
| BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry) |
Nylon 6, 40% Mineral Filled |
Ultramid®
|
| BASF Ultramid® 8260 HS PA6 (Conditioned) |
Nylon 6, 40% Mineral Filled |
Ultramid®
|
| BASF Ultramid® 8260 HS PA6 (Dry) |
Nylon 6, 40% Mineral Filled |
Ultramid®
|
| BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Conditioned) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Conditioned) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) |
Nylon 6, Glass/Mineral Reinforced |
Ultramid®
|
| BASF Ultramid® 8270 HS BK 102 PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8270 HS PA6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8270 HS PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) |
Nylon 6, 10% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8281 HS GP PA6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8281 HS GP PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® 8350 HS BK-102 PA6 (Conditioned) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8350 HS BK-102 PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8350 HS PA6 (Conditioned) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8350 HS PA6 (Dry) |
Nylon 6, Impact Grade |
Ultramid®
|
| BASF Ultramid® 8351 HS BK 102 PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8351 HS BK 106 PA6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® 8351 HS BK 106 PA6 (Dry) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B24 N 03 PA6 |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B24 NSD 05 PA6 |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B27 03 PA6 |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B27 E 01 PA6 (Conditioned) |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B27 E PA6 |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B27 SD 05 PA6 |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B36 LNV PA6 |
Nylon 6, Unreinforced |
Ultramid®
|
| BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) |
Nylon 6, 30% Glass Fiber Filled |
Ultramid®
|
| BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) |
Nylon 6, 40% Glass Fiber Filled |
Ultramid®
|