| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.291 g/cc | 0.04664 lb/in³ | Melt; ISO 1183 |
| 1.49 g/cc | 0.0538 lb/in³ | dry; ISO 1183 | |
| Water Absorption | 5.7 % | 5.7 % | beginning dry; ISO 62 |
| Moisture Absorption at Equilibrium | 1.6 % | 1.6 % | beginning dry (23°C/50% R.H.); ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 60.0 MPa | 8700 psi | 5mm/min; ISO 527 |
| Elongation at Break | 30 % | 30 % | 5mm/min; ISO 527 |
| Tensile Modulus | 2.39 GPa | 347 ksi | 1mm/min; ISO 527 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 1.999 J/g-°C | 0.4778 BTU/lb-°F | Melt |
| Thermal Conductivity | 0.281 W/m-K | 1.95 BTU-in/hr-ft²-°F | Melt |
| Melting Point | 220 °C | 428 °F | 10 K/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 275 °C | 527 °F | Injection molding |
| Mold Temperature | 95.0 °C | 203 °F | Injection molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Pellets | |
| Processing | Injection Molding | |
| Special characteristic | Heat stabilized or stable to heat | |